Mechanical Properties Metric English Comments
Tensile Strength, Yield 100 MPa

@Strain 0.200 %,
Temperature 300 °C
14500 psi

@Strain 0.200 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4306 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 100 MPa

@Strain 0.200 %,
Temperature 300 °C
14500 psi

@Strain 0.200 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel
General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll..
Tensile Strength, Yield 100 MPa

@Strain 0.200 %,
Temperature 500 °C
14500 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4401 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 100 MPa

@Strain 0.200 %,
Temperature 500 °C
14500 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4435 Cr-Ni-Mo Austenitic Stainless Steel
Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar, and rod forms..
Tensile Strength, Yield 100 MPa

@Strain 0.200 %,
Temperature 500 °C
14500 psi

@Strain 0.200 %,
Temperature 932 °F
EN min.; EN 10002-5
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel
General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r..
Tensile Strength, Yield 100 MPa

@Strain 0.200 %,
Temperature 300 °C
14500 psi

@Strain 0.200 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4828 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Yield 100 MPa

@Strain 0.200 %,
Temperature 300 °C
14500 psi

@Strain 0.200 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4833 High Temperature Austenitic Stainless Steel
Standardized high temperature steel for service at temperatures of up to 950-1000°C in dry air. Utilization in the temperature range of 600-900°C can lead to embrittlement.Applications: Heat and ..
Tensile Strength, Yield 100 MPa

@Strain 0.200 %,
Temperature 300 °C
14500 psi

@Strain 0.200 %,
Temperature 572 °F
EN min.; EN 10002-5
Outokumpu 4845 High Temperature Austenitic Stainless Steel
Standardized high-temperature steel for use at temperatures up to 1100°C in dry air. Prone to embrittlement after exposure between 600-900°C. Applications: Heat and creep resistance. For use o..
Tensile Strength, Yield >= 100 MPa

@Temperature 250 °C
>= 14500 psi

@Temperature 482 °F
PEAK Werkstoff DISPAL S250 Aluminum Alloy, AlSi20Fe5Ni2, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength, Yield 100 - 110 MPa

@Temperature 23.0 °C
14500 - 16000 psi

@Temperature 73.4 °F
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:..
Tensile Strength, Yield 100 MPa

@Temperature -40.0 °C
14500 psi

@Temperature -40.0 °F
ASTM D638
BASF Ultramid® 8281 HS GP PA6 (Conditioned)
Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p..