Material Notes:
Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering properties including strength, stiffness, and toughness combined with excellent abrasion resistance and self lubricating characteristics. In addition, the heat stabilizer system extends its retention of properties at elevated temperatures. Chemical resistance is excellent to greases, oils and hydrocarbons. All data is from injection molded specimens with the exception of Drop Weight Impact.Applications: Ultramid 8281 HS GP is generally recommended for applications such as fuel tanks, chemical storage tanks, hydraulic oil reservoirs, cyclones, and heat resistance containers.Information provided by BASF
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
ASTM D792
Moisture Absorption at Equilibrium 1.3 %
1.3 %
24 Hours; ASTM D570
2.7 %
2.7 %
50% RH; ASTM D570
9.5 %
9.5 %
Saturation; ASTM D570
Linear Mold Shrinkage 0.0508 cm/cm
0.0508 in/in
1/8" bar
Mechanical Properties Metric English Comments
Tensile Strength, Yield 33.0 MPa

@Temperature 23.0 °C
4790 psi

@Temperature 73.4 °F
ASTM D638
100 MPa

@Temperature -40.0 °C
14500 psi

@Temperature -40.0 °F
ASTM D638
Elongation at Break >= 100 %
>= 100 %
ASTM D638
Flexural Strength 32.0 MPa

@Temperature 23.0 °C
4640 psi

@Temperature 73.4 °F
ASTM D790
145 MPa

@Temperature -40.0 °C
21000 psi

@Temperature -40.0 °F
ASTM D790
Flexural Modulus 0.685 GPa

@Temperature 23.0 °C
99.4 ksi

@Temperature 73.4 °F
ASTM D790
2.26 GPa

@Temperature -40.0 °C
328 ksi

@Temperature -40.0 °F
ASTM D790
Processing Properties Metric English Comments
Dry Time 2 - 4 hour
2 - 4 hour
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Commercial Status North America