Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 86.0 MPa @Temperature 200 °C |
>= 12500 psi @Temperature 392 °F |
|
PEAK Werkstoff DISPAL S225 Aluminum Alloy, AlSi35Fe2Ni, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength, Yield | 86.2 MPa @Thickness 1.57 mm |
12500 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP344 Cotton Fabric Description: Fine weave canvas laminate with high temperature phenolic resin and molybdenum disulfide lubricant. Good machining properties and low coefficient of thermal expansion. Better machining .. |
|||
Tensile Strength, Yield | 86.2 MPa @Thickness 1.57 mm |
12500 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP615 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. NP615 is produced with high resin content melamine impregnated .. |
|||
Tensile Strength, Yield | 86.2 MPa @Thickness 1.57 mm |
12500 psi @Thickness 0.0620 in |
LW; ASTM D638 |
Industrial Laminates/Norplex NP612 Paper Base Laminate Description: Room temperature punching and shearing grade up to .125" thick. More flexible and lower mechanical properties than NP611. Intended for applications where electrical and moisture require.. |
|||
Tensile Strength, Yield | 86.2 MPa @Thickness 1.57 mm |
12500 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP664 Paper Base Laminate Description: Low cost room temperature punching grade with mechanical and electrical properties similar to NP612. This version is made with pigment cover plies on the surface.Thickness Tested: 0.062.. |
|||
Tensile Strength, Yield | 86.2 MPa @Thickness 1.57 mm |
12500 psi @Thickness 0.0620 in |
CW; ASTM D638 |
Industrial Laminates/Norplex NP321 Cotton Fabric
(discontinued **) Description: NP321 consists of a fine weave cotton fabric (linen) impregnated with a phenolic resin binder. Applications include vanes for air and liquid pumps, and compressors. NP321 remains very f.. |