Mechanical Properties | Metric | English | Comments |
---|---|---|---|
K (wear) Factor | 5040 x 10-8 mm³/N-M | 2500 x 10-10 in³-min/ft-lb-hr | |
Greene Tweed Avalon® 1 PTFE Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin.. |
|||
K (wear) Factor | 5040 x 10-8 mm³/N-M | 2500 x 10-10 in³-min/ft-lb-hr | |
Greene Tweed Avalon® 56 PTFE PTFE is used in many pharmaceutical-sealing applications. Its chemical inertness and ultra-low level extractables provide pharmaceutical process and validation engineers with a safe material to use.. |
|||
K (wear) Factor | 5040 x 10-8 mm³/N-M | 2500 x 10-10 in³-min/ft-lb-hr | 40 psi, 50 fpm; ASTM D3702 |
Ensinger Tecanat™ Unfilled Polycarbonate (PC) Tenacat™ is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps.. |