Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ensinger Tecanat™ Unfilled Polycarbonate (PC)

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, Molded
Manufacturer Ensinger
Trade Name Tecanat™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ensinger Tecanat™ Unfilled Polycarbonate (PC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Tenacat™ is typically used in business equipment where gears, rollers, interlam mechanical parts, connectors and relays are required. The automotive industry uses polycarbonate materials for pumps, valves, light bezels and instrument panels. Excellent dimensional stability Transparency Good machinabilityInformation provided by Ensinger, Inc.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ASTM D792
Water Absorption 0.15 %
0.15 %
at 24 hours; ASTM D570
Water Absorption at Saturation 0.35 %
0.35 %
ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 70
70
ASTM D785
Hardness, Rockwell R 118
118
ASTM D785
Tensile Strength, Yield 60.0 MPa
8700 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Tensile Modulus 2.07 GPa
300 ksi
ASTM D638
Flexural Strength 97.9 MPa
14200 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
ASTM D256
Coefficient of Friction, Dynamic 0.38
0.38
40 psi, 50 fpm; ASTM D3702
K (wear) Factor 5040 x 10-8 mm³/N-M
2500 x 10-10 in³-min/ft-lb-hr
40 psi, 50 fpm; ASTM D3702
Thermal Properties Metric English Comments
CTE, linear 68.4 µm/m-°C

@Temperature 20.0 °C
38.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Specific Heat Capacity 1.26 J/g-°C
0.300 BTU/lb-°F
Maximum Service Temperature, Air 116 °C
240 °F
Long Term; ASTM UL746B
135 °C
275 °F
Intermittent
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 132 °C
270 °F
ASTM D648
Vicat Softening Point 154 °C
310 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 2.96

@Frequency 1e+6 Hz
2.96

@Frequency 1e+6 Hz
ASTM D150
3.2

@Frequency 60 Hz
3.2

@Frequency 60 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
380 kV/in
ASTM D149
Dissipation Factor 0.00090

@Frequency 60 Hz
0.00090

@Frequency 60 Hz
ASTM D150