Mechanical Properties Metric English Comments
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Ring; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP DFL36P PC
LNP* Lubricomp* DFL36P is a compound based on Polycarbonate containing 30% Glass Fiber 15% PTFE. Added features include: Exceptional Processing. Internally Lubricated.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Dry: 0.25 m/s, 3.4 MPa (50 fpm, 500 psi); ASTM D3702
Solvay Specialty Polymers Torlon® 4301 Polyamide-imide (PAI)  (Unverified Data**)
Torlon 4301 is a wear-resistant grade of polyamide-imide (PAI) resin. It has a good balance of mechanical properties and wear resistance. It offers high flexural and compressive strength with a low ..
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP ICL34 PA6.12
LNP* LUBRICOMP* ICL34 is a compound based on Nylon 6/12 containing 20% Carbon Fiber, 15% PTFE. Added features include: Wear Resistant.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP KL003LH Acetal
LNP* LUBRICOMP* KL003LH is an Acetal based compound containing 15% PTFE. Added features of this grade include: Low Extractable, Healthcare, Wear Resistant.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP LCL33EXQ PEEK
LNP* LUBRICOMP* LCL33EXQ is a compound based on Polyetheretherketone containing 15% Carbon Fiber, 15% PTFE. Added features of this material include: Wear Resistant, Easy Molding.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6
LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP SCP36 PA12
LNP* LUBRICOMP* SCP36 is a compound based on Nylon 12 containing 30% Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Wear Resistant, Electrically Conductive.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP SFP36 PA12
LNP* LUBRICOMP* SFP36 is a compound based on Nylon 12 resin containing 30% Glass Fiber 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP THERMOCOMP RC008 PA 66
LNP THERMOCOMP* RC008 is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly
LNP* STAT-LOY* K3000SZ is a compound based on Acetal Copolymer resin. Added feature of this material is: AntiSstatic.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP STAT-LOY K3000SZ Acetal Copoly (Asia Pacific)
LNP* Stat-loy* K3000SZ is a compound based on Acetal Copolymer resin containing Anti-Static. Added features of this material include: Antistat.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP STAT-LOY K3000Z Acetal
LNP* STAT-LOY* K3000Z is a compound based on unfilled Acetal resin. Added feature of this material is: Antistat.
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
K=W/PVT where W=wear (inches^3); P=applied pressure (psi); V=velocity (fpm); T=time (hours).
A. Schulman ComAlloy E-13370B Internally Lubricated, Glass Fiber Reinforced Polyester Alloy
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
K (wear) Factor 28.2 x 10-8 mm³/N-M
14.0 x 10-10 in³-min/ft-lb-hr
K=W/PVT where W=wear (inches^3); P=applied pressure (psi); V=velocity (fpm); T=time (hours).
A. Schulman ComAlloy Lubrilon® 629 Nylon 6/6, Glass Fiber/PTFE Filled, Flow Enhanced
Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma..
Copyright © lookpolymers.com All Rights Reserved