Polymer Property : K (wear) Factor = 117 x 10-8 mm³/N-M Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
K (wear) Factor 117 x 10-8 mm³/N-M
58.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11
LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing 25% Glass Fiber, 10% Graphite. Added features of this material include: Internally Lubricated.
K (wear) Factor 117 x 10-8 mm³/N-M
58.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific)
LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated.
K (wear) Factor 117 x 10-8 mm³/N-M
58.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP JFL34 PES
LNP* LUBRICOMP* JFL34 is a compound based on Polyethersulfone resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
K (wear) Factor 117 x 10-8 mm³/N-M
58.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT
LNP LUBRICOMP* WL004 is a compound based on PBT resin containing 20% PTFE. Added features of this material include: Wear Resistant.
K (wear) Factor 117 x 10-8 mm³/N-M
58.0 x 10-10 in³-min/ft-lb-hr
Washer; ASTM D3702 Modified
SABIC Innovative Plastics LNP LUBRICOMP WL004 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WL004 is a compound based on Polybutylene Terephalate resin containing PTFE.
K (wear) Factor 117 x 10-8 mm³/N-M
58.0 x 10-10 in³-min/ft-lb-hr
Techmer ES Luriblend® PC MRX BK