Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Techmer ES Luriblend® PC MRX BK

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Techmer ES
Trade Name Luriblend®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Luriblend® PC MRX BK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0080 cm/cm

@Thickness 3.17 mm
0.0080 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 59.3 MPa
8600 psi
ASTM D638
Elongation at Yield 90 %
90 %
ASTM D638
Flexural Yield Strength 83.4 MPa
12100 psi
ASTM D790
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm

@Thickness 3.17 mm
15.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched NB

@Thickness 3.17 mm
NB

@Thickness 0.125 in
ASTM D256
Coefficient of Friction, Dynamic 0.090
0.090
ASTM D1894
Coefficient of Friction, Static 0.060
0.060
ASTM D1894
K (wear) Factor 117 x 10-8 mm³/N-M
58.0 x 10-10 in³-min/ft-lb-hr
Limiting Pressure Velocity 0.788 MPa-m/sec
22500 psi-ft/min
10 fpm
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 68.4 µm/m-°C
38.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 138 °C
280 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 127 °C
260 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved