Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 980 MPa | 142000 psi | ASTM D790 |
Flint Hills P5M6N-058A Polypropylene Random Copolymer Features: Excellent processabilty, nucleated and antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: consumer disposable itemsInformation .. |
|||
Flexural Modulus, 1% Secant | 980 MPa | 142000 psi | ASTM-D790 |
Braskem AD57 HDPE Monofilament Polyethylene Copolymer AD57 resin is a high-density polyethylene, copolymer of butene-1, produced by the solution process, designed for raffia extrusion, and Raschel knitted with excellent optical and mechanical propertie.. |
|||
Flexural Modulus, 1% Secant | 980 MPa | 142000 psi | ASTM-D790 |
Braskem GF5250 HDPE Blow Molding Polyethylene Copolymer GF5250 is a high-density polyethylene copolymer with well balanced properties between impact and stiffness combined with high productivity and good processability. It was developed for the blow-mold.. |
|||
Flexural Modulus, 1% Secant | 980 MPa | 142000 psi | ASTM-D790 |
Braskem GM5240PR HDPE High Density Extrusion Polyethylene GM5240PR is a high-density polyethylene compound specially developed for the manufacturing of pipes, underground conduits, and steel pipe coating. This resin is produced with bimodal technology and .. |
|||
Flexural Modulus, 1% Secant | 980 MPa | 142000 psi | ASTM D790 |
Braskem GM5340PR High Density Polyethylene Triple-layer coating for metallic pipes; Umbilical pipes for offshore oil field platforms; Jacketing for wires and for optic fiber metallic cables; Self-propelled irrigation pipes; Localized irrigat.. |