Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Flint Hills P5M6N-058A Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Flint Hills Resources
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P5M6N-058A Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: Excellent processabilty, nucleated and antistat. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: consumer disposable itemsInformation Provided by Flint Hills Resources
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 35 g/10 min
35 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 89
89
ASTM D785
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus, 1% Secant 980 MPa
142000 psi
ASTM D790
Izod Impact, Notched 0.400 J/cm

@Temperature 23.0 °C
0.749 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Gardner Impact >= 36.0 J

@Temperature 23.0 °C
>= 26.6 ft-lb

@Temperature 73.4 °F
ASTM D5420
Tangent Modulus 990 MPa
144000 psi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 91.0 °C
196 °F
ASTM D648