Braskem AD57 HDPE Monofilament Polyethylene Copolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , HDPE, Fiber Grade
Manufacturer Braskem
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem AD57 HDPE Monofilament Polyethylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AD57 resin is a high-density polyethylene, copolymer of butene-1, produced by the solution process, designed for raffia extrusion, and Raschel knitted with excellent optical and mechanical properties, associated with good processability. It contains antioxidant additives. Its applications include: Raschel knitted, raffia extrusion, tarpaulin, general use, monofilaments, and oriented structures. Processing Conditions for Oriented Structures: cast film - typical temperature profile: 190 to 230ºC; blown film - typical temperature profile: 190 to 215ºC; monofilament - typical temperature profile: 190 to 230ºC. Typical Stretch Ratio: 6 to 8:1.
Physical Properties Metric English Comments
Density 0.951 g/cc
0.0344 lb/in³
ASTM-D792
Melt Flow 0.60 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.60 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 56
56
ASTM-D2240
Tensile Strength at Break 35.0 MPa
5080 psi
ASTM-D638
Tensile Strength, Yield 25.0 MPa
3630 psi
ASTM-D638
Elongation at Break 2044 %
2044 %
ASTM-D638
Elongation at Yield 12 %
12 %
ASTM-D638
Flexural Modulus, 1% Secant 980 MPa
142000 psi
ASTM-D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C
151 °F
ASTM-D648
Vicat Softening Point 125 °C

@Load 1.02 kg
257 °F

@Load 2.25 lb
ASTM-D1525