Polymer Property : Flexural Modulus, 1% Secant = 875 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 875 MPa
127000 psi
ASTM D790
Flint Hills P6E2A-005 Impact Copolymer Polypropylene
Impact copolymer, UL certified.Features: LTHA and extra high impact strength.Applications: Injection molding and extrusion: high pressure resistance, film, and flexible profiles.Former Huntsman poly..