Flint Hills P6E2A-005 Impact Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P6E2A-005 Impact Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact copolymer, UL certified.Features: LTHA and extra high impact strength.Applications: Injection molding and extrusion: high pressure resistance, film, and flexible profiles.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 1.8 g/10 min
1.8 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 58
58
ASTM D785
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 0.925 GPa
134 ksi
Tangent; ASTM D790
Flexural Modulus, 1% Secant 875 MPa
127000 psi
ASTM D790
Izod Impact, Notched NB
NB
ASTM D256
Gardner Impact >= 36.0 J

@Temperature -30.0 °C
>= 26.6 ft-lb

@Temperature -22.0 °F
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648
Flammability, UL94 HB
HB