Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 875 MPa | 127000 psi | ASTM D790 |
Flint Hills P6E2A-005 Impact Copolymer Polypropylene Impact copolymer, UL certified.Features: LTHA and extra high impact strength.Applications: Injection molding and extrusion: high pressure resistance, film, and flexible profiles.Former Huntsman poly.. |