Polymer Property : Flexural Modulus, 1% Secant = 35000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus, 1% Secant 241 MPa
35000 psi
ASTM D790
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin
Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Availability: Latin America, North ..