Material Notes:
Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Availability: Latin America, North America and South AmericaApplications: Crosslinkable CompoundsWire and Cable CompoundsInformation provided by ExxonMobil
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ExxonMobil method
Melt Flow 2.3 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.3 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 90

@Time 15.0 sec
90

@Time 0.00417 hour
ASTM D2240
Hardness, Shore D 44

@Time 15.0 sec
44

@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break 10.3 MPa
1500 psi
ASTM D638
Tensile Strength, Yield 11.7 MPa
1700 psi
ASTM D638
Elongation at Break 630 %
630 %
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus, 1% Secant 241 MPa
35000 psi
ASTM D790
Thermal Properties Metric English Comments
Melting Point <= 228 °C
<= 442 °F
Peak Melting Point; ExxonMobil method
Electrical Properties Metric English Comments
Volume Resistivity 7.60e+15 ohm-cm
7.60e+15 ohm-cm
ASTM D257
Dielectric Constant 2.3
2.3
ASTM D150
Dielectric Strength 51.2 kV/mm
1300 kV/in
ASTM D149
Dissipation Factor 0.000080
0.000080
ASTM D150