Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus, 1% Secant | 241 MPa | 35000 psi | ASTM D790 |
ExxonMobil LDPE LD 419.MV Low Density Polyethylene Resin Product Description: LD 419.MV is a LDPE designed for wire and cable applications and is suitable for making crosslinkable compounds for medium voltage insulation.Availability: Latin America, North .. |