Braskem AC59 HDPE Monofilament Polyethylene Homopolymer

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , HDPE, Fiber Grade
Manufacturer Braskem
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Braskem AC59 HDPE Monofilament Polyethylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AC59 resin is a high-density polyethylene homopolymer produced by the solution process and designed for monofilament applications. It contains antioxidant additives. Its applications include: film extrusion, monofilament, raffia, raschel, nets, oriented structures, and general use. Processing Conditions for Oriented Structures: cast film - typical temperature profile: 170 to 220ºC; blown film - typical temperature profile: 170 to 220ºC; monofilament - typical temperature profile: 170 to 220ºC. Typical Stretch Ratio: 4 to 8:1.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
ASTM-D792
Melt Flow 0.75 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.75 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
ASTM-D2240
Tensile Strength at Break 35.0 MPa
5080 psi
ASTM-D638
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM-D638
Elongation at Break 2036 %
2036 %
ASTM-D638
Elongation at Yield 11 %
11 %
ASTM-D638
Flexural Modulus, 1% Secant 1180 MPa
171000 psi
ASTM-D790
Izod Impact, Notched 1.75 J/cm
3.28 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ASTM-D648
Vicat Softening Point 127 °C

@Load 1.02 kg
261 °F

@Load 2.25 lb
ASTM-D1525