Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 87.0 MPa @Temperature 300 °C |
>= 12600 psi @Temperature 572 °F |
|
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational.. |
|||
Tensile Strength at Break | 87.0 MPa @Temperature 23.0 °C |
12600 psi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66
(Unverified Data**) Minlon® 11C140 BK086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 87.0 MPa @Temperature 23.0 °C |
12600 psi @Temperature 73.4 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Strength at Break | 87.0 MPa @Temperature 250 °C |
12600 psi @Temperature 482 °F |
ISO 527-1 |
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex.. |