Mechanical Properties Metric English Comments
Tensile Strength at Break >= 87.0 MPa

@Temperature 300 °C
>= 12600 psi

@Temperature 572 °F
PEAK Werkstoff DISPAL S260 Aluminum Alloy, AlSi25Cu4Mg, Condition F
Excellent properties:abrasive stabilityhigh stiffness (E-modulus)resistance even at high temperaturesgood grindabilityPEAK DISPAL materials allow the manufacturing of pistons for highest operational..
Tensile Strength at Break 87.0 MPa

@Temperature 23.0 °C
12600 psi

@Temperature 73.4 °F
DAM; ISO 527
DuPont Performance Polymers Minlon® 11C140 BK086 Nylon 66  (Unverified Data**)
Minlon® 11C140 BK086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers
Tensile Strength at Break 87.0 MPa

@Temperature 23.0 °C
12600 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66  (Unverified Data**)
Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 87.0 MPa

@Temperature 250 °C
12600 psi

@Temperature 482 °F
ISO 527-1
Vyncolit Neopreg Kinel® SK4502 S8 Carbon Reinforced Molding Compound
KINEL SK4502 S8 is a long carbon fiber reinforced BMI molding compound suited for very demanding tribological applications, high speeds and temperatures even under dry running conditions. Thermal ex..