Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 9.50 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
4.52 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² @Temperature -30.0 °C |
4.52 ft-lb/in² @Temperature -22.0 °F |
ISO 180/1A |
Nilit Nilamid B3 H G6 30% Glass Fiber Reinforced PA6 Description: Nilamid B3 H G6 is a general purpose, 30% glass fiber reinforced NYLON 6 with a combination of good mechanical performance, impact strength and processability. It is one of the most wid.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
4.52 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180/1A |
Polimeri Europa Sinkral® D 232/M3 ABS Resin
(discontinued **) Special low gloss extrusion/ co-extrusion grade, with good flow. Designation: Thermoplastic ISO 2580-ABS 1, EGN, 105-08-09-15Applications: Sinkral D 232-M3 is widely used in the extrusion / co-extr.. |
|||
Izod Impact, Notched (ISO) | 9.50 kJ/m² @Temperature 23.0 °C |
4.52 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |