Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 8.20 kJ/m² @Temperature -40.0 °C |
3.90 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
NOVA Chemicals Dylark® 378P15 Glass Reinforced Engineering Resin Features: Very high modulus, High heat resistance, excellent flow characteristics, excellent adhesion to urethaneApplications: Instrument panel substrates, Consoles, Cluster housings, Interior trim |
|||
Izod Impact, Notched (ISO) | 8.20 kJ/m² @Temperature 23.0 °C |
3.90 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Izod Impact, Notched (ISO) | 8.19 kJ/m² @Temperature 22.8 °C |
3.90 ft-lb/in² @Temperature 73.0 °F |
ISO 180/1A |
ExxonMobil AP3N Polypropylene Impact Copolymer Product Description: A medium impact copolymer resin designed for appliance applications requiring good stiffness and fast cycle time.Availability: Asia Pacific Features:Fast Molding CycleHigh Glos.. |