Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.36 kJ/m² @Temperature -40.0 °C |
1.60 ft-lb/in² @Temperature -40.0 °F |
ISO 180/1A |
ExxonMobil AP3AW Polypropylene Impact Copolymer Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe.. |