Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.36 kJ/m²

@Temperature -40.0 °C
1.60 ft-lb/in²

@Temperature -40.0 °F
ISO 180/1A
ExxonMobil AP3AW Polypropylene Impact Copolymer
Product Description: A UV stabilized medium impact copolymer resin designed for automotive battery cases.Availability: Asia Pacific Features:Good UV ResistanceHigh StiffnessLow WarpageMedium FlowMe..