Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.20 kJ/m² @Temperature -40.0 °C |
1.52 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CB247G Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB247G high melt flow, 1,700 MPa flexural modulus, UV-stabilized, weatherable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of propert.. |
|||
Izod Impact, Notched (ISO) | 3.20 kJ/m² @Temperature -40.0 °C |
1.52 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ CB276 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ CB276 very high melt flow, 1,200 MPa flexural modulus, UV-stabilized, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of .. |