Izod Impact, Notched (ISO) 3.20 kJ/m²

@Temperature -40.0 °C
1.52 ft-lb/in²

@Temperature -40.0 °F
ISO 180
LyondellBasell Hifaxâ„¢ CB247G Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB247G high melt flow, 1,700 MPa flexural modulus, UV-stabilized, weatherable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of propert..
Izod Impact, Notched (ISO) 3.20 kJ/m²

@Temperature -40.0 °C
1.52 ft-lb/in²

@Temperature -40.0 °F
ISO 180
LyondellBasell Hifaxâ„¢ CB276 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CB276 very high melt flow, 1,200 MPa flexural modulus, UV-stabilized, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of ..