Polymer Property : Izod Impact, Notched (ISO) = 9.80 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 6.40 - 9.80 kJ/m²
3.05 - 4.66 ft-lb/in²
Average value: 8.53 kJ/m² Grade Count:3
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum..