Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 6.40 - 9.80 kJ/m² | 3.05 - 4.66 ft-lb/in² | Average value: 8.53 kJ/m² Grade Count:3 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |