Polymer Property : Izod Impact, Notched (ISO) = 7.40 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 7.40 kJ/m²
3.52 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)  (Unverified Data**)
AV-722 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding wea..
Izod Impact, Notched (ISO) 7.40 kJ/m²
3.52 ft-lb/in²
ISO 180
Solvay Specialty Polymers AvaSpire® AV-722 SL30 Polyaryletherketone (PAEK)
AV-722 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to the outstanding..
Izod Impact, Notched (ISO) 7.40 kJ/m²
3.52 ft-lb/in²
ISO 180-A
Ecomass® 3011ZD86 Tungsten Filled Polycarbonate
Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsHigh Specific GravityTungsten Filled Polycarbonate (PC) CompoundGood ToughnessInformation provided by Tech..
Izod Impact, Notched (ISO) 7.40 kJ/m²
3.52 ft-lb/in²
ISO 180-A
Ecomass® 4450CI86 Carbonyl Iron Filled Polypropylene
Nontoxic alternative to Lead (Pb), for shielding applicationsHigh Specific GravityCarbonyl Iron Filled Polypropylene Random Co-PolymerInformation provided by Technical Polymers
Izod Impact, Notched (ISO) 7.40 kJ/m²

@Thickness 3.20 mm
3.52 ft-lb/in²

@Thickness 0.126 in
ISO 180-A
Ecomass® 705ZC75 Stainless Steel Filled ABS
Nontoxic Alternative to traditional metals, weighting and balancing applicationsModerate Specific GravityStainless Steel Powder Filled ABSInformation provided by Technical Polymers
Izod Impact, Notched (ISO) 7.40 kJ/m²
3.52 ft-lb/in²
ISO 180
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..