Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ecomass® 4450CI86 Carbonyl Iron Filled Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Ecomass Technologies
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ecomass® 4450CI86 Carbonyl Iron Filled Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Nontoxic alternative to Lead (Pb), for shielding applicationsHigh Specific GravityCarbonyl Iron Filled Polypropylene Random Co-PolymerInformation provided by Technical Polymers
Physical Properties Metric English Comments
Specific Gravity 3.70 g/cc
3.70 g/cc
ASTM D792
Linear Mold Shrinkage 0.0060 - 0.010 cm/cm
0.0060 - 0.010 in/in
Internal
Mechanical Properties Metric English Comments
Tensile Strength at Break 19.0 MPa
2760 psi
ISO 527
Elongation at Break 1.3 %
1.3 %
ISO 527
Flexural Modulus 3.796 GPa
550.6 ksi
ISO 178
Izod Impact, Notched (ISO) 7.40 kJ/m²
3.52 ft-lb/in²
ISO 180-A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 76.0 °C
169 °F
ISO 75
Processing Properties Metric English Comments
Melt Temperature 200 - 215 °C
392 - 419 °F
Mold Temperature 10.0 - 38.0 °C
50.0 - 100 °F
Users viewing this material also viewed the following: