Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® 905 PC Copolymer (Asia Pacific)
Lexan 905 resin is a high flow, opaque, flame retardant polycarbonate resin blend. It is designed with non-chlorinated, non-brominated FR systems with UL-94 listing of both V0 and 5V ratings. Its ex..
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HPF0 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® ML7681 PC Copolymer (Asia Pacific)
Polycarbonate with high flow, good processability, good impact and thermal properties, non-Chlorine and non-Bromine flame retardant, UL rated V-0 and V-1. Available in limited translucent colors onl..
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP COLORCOMP D10006U PC
LNP* COLORCOMP* D10006U is an unfilled Polycarbonate. Added features include: Lasermarking Capability, UL Listed.
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1830 PC Copolymer (Europe-Africa-Middle East)
40 MFR LEXAN High Flow Ductile Copolymer UV Stabilized, available in transparent colors only
Izod Impact, Notched (ISO) 58.0 kJ/m²

@Temperature 23.0 °C
27.6 ft-lb/in²

@Temperature 73.4 °F
ISO 180/4A
Styron CALIBREâ„¢ 301-58 LT Polycarbonate Resin
Overview: CALIBREâ„¢ 301-58 LT is a high light transmission, high-flow polycarbonate resin for injection molding applications.Main Characteristics:High light transmissionHigh flow for injection m..
Izod Impact, Notched (ISO) 58.0 kJ/m²

@Temperature 0.000 °C
27.6 ft-lb/in²

@Temperature 32.0 °F
80*10*3; ISO 180/1A
SABIC Innovative Plastics Valox® V3903WX PBT+PC (Asia Pacific)
Unreinforced fllame retardant PBT/PC blends with good chemical resistance and low temperature impact, UV stablized
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer
40 MFR LEXAN High Flow Ductile Copolymer
Izod Impact, Notched (ISO) 58.0 kJ/m²
27.6 ft-lb/in²
80*10*3; ISO 180/1A
SABIC Innovative Plastics Lexan® HFD1810 PC Copolymer (Asia Pacific)
40 MFR LEXAN High Flow Ductile Copolymer
Copyright © lookpolymers.com All Rights Reserved