Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
Type A; ISO 180:2000
Nylacast Cast Nylon 6, Glass Filled
Information provided by Nylacast Ltd.
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
Type A; ISO 180:2000
Nylacast PA6C Cast Nylon 6
Natural PA6 is the base to the other grades of material offered by Nylacast. It is available in Natural (off white) or Black colour. It is made by ionic polymerisation of e-caprolactam under anhydri..
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
ISO 180
Polikim KESTAMID® PA6G Polyamide 6
Kestamid® is also known as Cast Polyamide or Cast Nylon. Kestamid® is an engineering plastic used commonly in all industrial branches for its superior mechanical, physical, chemical and electrical..
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
Sample Type A; ISO 180:2000
Global EPP PA 6C Cast Polyamide 6
Cast nylons are generally accepted as the primary engineering polymer, suitable for virtually any plain bearing application. By varying the conditions of polymerisation the mechanical properties of ..
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
ISO 180-93
Wellman EcoLon® MRGF1616-BK 40% Mineral/Glass Reinforced Post Consumer Compound Nylon 6
Description: Mineral/Glass Reinforced Post Consumer Compound Nylon 6Information provided by Wellman.
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.67 ft-lb/in²
1A; ISO 180
Azoty Tarnow™ TARNOFORM 300 M POM
Tribological modified grade with addition of molybdenum disulphide, which causes decreased coefficient of friction and wear, especially for applications requiring high load at low sliding speed.Info..
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
ISO 180
LNP Stat-Kon® SS- Polyamide 12, Stainless Steel Fiber  (discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
ISO 180
Polikim KESTAMID® HS Polyamide 6, Heat Resistant
Kestamid-HS® is Polikim’s cast polyamide with increased heat resistance. Thermal stabilizer additives increase thermal aging significantly. In operating temperatures over 80°C, it performs with ..
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
ISO 180
BASF Ultramid® B3WG3 15% Glass Filled PA6 (Dry)
Description: Ultramid B3WG3 is a 15% glass fiber reinforced, heat stabilized injection molding PA6 grade.Information provided by BASF
Copyright © lookpolymers.com All Rights Reserved