Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Ultramid® B3WG3 15% Glass Filled PA6 (Dry)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, 20% Glass Fiber Filled
Manufacturer BASF
Trade Name Ultramid®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Ultramid® B3WG3 15% Glass Filled PA6 (Dry).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultramid B3WG3 is a 15% glass fiber reinforced, heat stabilized injection molding PA6 grade.Information provided by BASF
Mechanical Properties Metric English Comments
Flexural Modulus 5.40 GPa
783 ksi
ISO 178
Izod Impact, Notched (ISO) 5.60 kJ/m²
2.66 ft-lb/in²
ISO 180
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
ISO 3146
UL RTI, Electrical 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
746B
UL RTI, Mechanical with Impact 85.0 °C

@Thickness 1.50 mm
185 °F

@Thickness 0.0591 in
746B
UL RTI, Mechanical without Impact 130 °C

@Thickness 1.50 mm
266 °F

@Thickness 0.0591 in
746B
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Processing Properties Metric English Comments
Melt Temperature 250 - 290 °C
482 - 554 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
Dry Time 2 - 4 hour
2 - 4 hour
Descriptive Properties Value Comments
Commercial Status North America
Users viewing this material also viewed the following: