Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 10.5 kJ/m²

@Temperature 23.0 °C
5.00 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
Izod Impact, Notched (ISO) 10.5 kJ/m²

@Temperature 23.0 °C
5.00 ft-lb/in²

@Temperature 73.4 °F
ISO 180/A
Victrex® PEEK 450CA30 30% Carbon Fiber Reinforced
General purpose, 30% carbon fiber reinforced, pelletized grade for injection molding.Information provided by Victrex.
Izod Impact, Notched (ISO) 10.5 kJ/m²
5.00 ft-lb/in²
ISO 180/A
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Izod Impact, Notched (ISO) 10.5 kJ/m²

@Temperature 23.0 °C
5.00 ft-lb/in²

@Temperature 73.4 °F
ISO 180
Victrex® PEEK 90HMF40 Polyetheretherketone (PEEK), 40% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 40% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, easy flow, color black.Typica..
Izod Impact, Notched (ISO) 10.5 kJ/m²
5.00 ft-lb/in²
ISO 180
LNP Thermocomp® EF-1006 BK8-114 Polyetherimide, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
Izod Impact, Notched (ISO) 10.5 kJ/m²
5.00 ft-lb/in²
ISO 180-93
Wellman Wellamid® GF1497-BK 43% Glass Fiber Reinforced, Silicone Lubricated Nylon 66
Description: Glass Fiber Reinforced, Silicone Lubricated Nylon 66Information provided by Wellman.
Izod Impact, Notched (ISO) 10.5 kJ/m²
5.00 ft-lb/in²
ISO 180
Polyram PlusTek RA301G8 Nylon 6.6 for Injection Molding, 40% Glass Fiber Reinforced, Heat Stabilized
Heat stabilized, 40% glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram.
Izod Impact, Notched (ISO) 10.5 kJ/m²
5.00 ft-lb/in²
Conditioned; ISO 180/1A
Addiplast Addilene J 690 RM20F Flame Retardant Polypropylene, 20% Mineral Filled
Flame retardant, mineral filled, with halogens, impact resistantInformation provided by Addiplast.
Izod Impact, Notched (ISO) 10.5 kJ/m²

@Temperature -20.0 °C
5.00 ft-lb/in²

@Temperature -4.00 °F
ASTM D256
C.O.I.M. LARIPUR® LPR5760 PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Izod Impact, Notched (ISO) 10.5 kJ/m²
5.00 ft-lb/in²
Conditioned; ISO 180/1A
Addiplast Addinyl A2H V25 Flame Retardant Nylon 66, 25% Glass Filled
Flame retardant, 25% glass fiber reinforced, with halogensInformation provided by Addiplast.