Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.90 kJ/m²
2.33 ft-lb/in²
ISO 180
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)  (Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
Izod Impact, Notched (ISO) 4.90 - 11.0 kJ/m²
2.33 - 5.23 ft-lb/in²
Average value: 8.03 kJ/m² Grade Count:3
Overview of materials for Polycarbonate, Stainless Steel Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Stainless Steel Fiber". Each property range of values reported is minimum and maximum val..
Izod Impact, Notched (ISO) 4.90 kJ/m²
2.33 ft-lb/in²
ISO 180
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
Izod Impact, Notched (ISO) 4.90 kJ/m²
2.33 ft-lb/in²
ISO 180
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
Izod Impact, Notched (ISO) 4.90 kJ/m²
2.33 ft-lb/in²
ISO 180-93
Wellman Wellamid® MRGFX1393-N 40% Mineral/Glass Reinforced, Silicone Lubricated Nylon 6
Description: Mineral/Glass Reinforced, Silicone Lubricated Nylon 6Information provided by Wellman.