Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 2.90 - 170 kJ/m² | 1.38 - 80.9 ft-lb/in² | Average value: 24.1 kJ/m² Grade Count:23 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Izod Impact, Notched (ISO) | 2.90 kJ/m² | 1.38 ft-lb/in² | ISO 180/1A |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA)
(Unverified Data**) Amodel A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over a b.. |
|||
Izod Impact, Notched (ISO) | 2.90 kJ/m² | 1.38 ft-lb/in² | ISO 180 |
MRC Polymers MAXTEL™ 650-BK Polypropylene Homopolymer • For injection molding• Excellent process ability with high flow.Information provided by MRC Polymers Inc. |
|||
Izod Impact, Notched (ISO) | 2.90 kJ/m² | 1.38 ft-lb/in² | Type 1, Notch A; ISO 180 |
Solvay Specialty Polymers Amodel® A-4422 LS WH118 Polyphthalamide (PPA), 22% Mineral Amodel® A-4422 LS resin is a 22% reinforced, light-stabilized, high-reflectivity white grade of polyphthalamide (PPA). The material exhibits high heat resistance, high strength and stiffness over.. |
|||
Izod Impact, Notched (ISO) | 2.90 kJ/m² | 1.38 ft-lb/in² | 80x10x4; ISO 180/1A |
Eurostar Starpylen HZ 50E3 PP, Injection Molded PRELIMINARY-Starpylen HZ 50E3 is a High Specific Gravity Polypropylene (density 1.5), Injection Molding Resin (also known as HZ50E3)Information provided by Eurostar. |
|||
Izod Impact, Notched (ISO) | 2.90 kJ/m² | 1.38 ft-lb/in² | ISO 180/1A |
A.D. Compound Adene NTQA Homopolymer 40% Talc Filled Polypropylene Information provided by A.D. Compound |