Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.90 - 170 kJ/m²
1.38 - 80.9 ft-lb/in²
Average value: 24.1 kJ/m² Grade Count:23
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..