Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.20 - 35.0 kJ/m² | 2.47 - 16.7 ft-lb/in² | Average value: 10.8 kJ/m² Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Izod Impact, Notched (ISO) | 8.00 - 35.0 kJ/m² | 3.81 - 16.7 ft-lb/in² | Average value: 18.7 kJ/m² Grade Count:3 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |