Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | ISO 180 |
LNP Stat-Kon® OC-1006 Polyphenylene Sulfide, Carbon Fiber Reinforcement
(discontinued **) Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades.. |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² @Temperature -40.0 °C |
2.47 ft-lb/in² @Temperature -40.0 °F |
ISO 180 |
Phillips Sumika Marlex® CHP-275 Thermoplastic Polyolefin
(discontinued **) Engineered Thermoplastic Polyolefin.Applications: Automotive Head and Side Impact TrimConditioning after Molding: 48 hr at 23°C, 48 hr at 90°CNominal Shrinkage: 0.7-0.9%, 0.8-1.1%Drying conditions.. |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | ISO 180 |
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Izod Impact, Notched (ISO) | 5.20 - 35.0 kJ/m² | 2.47 - 16.7 ft-lb/in² | Average value: 10.8 kJ/m² Grade Count:7 |
Overview of materials for Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler". Specific grades with glass content between 15%.. |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | ISO 180/1A |
Lucite International Diakon® TD542 Toughened Acrylic Compound The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by.. |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | 1A; ISO 180 |
Azoty Tarnow™ TARNOFORM 300 GF6 BK POM 30% glass fiber reinforced injection molding grade, suitable for applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A... |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | ISO Test |
BASF Ultramid® 1403-2 BK ND3007 PA66 (Dry) |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | ISO Test |
BASF Ultramid® 1403-2 NF3001 13% Glass Filled PA66 (Dry) Ultramid 1403-2 NF3001 is a 13% glass reinforced, heat stabilized injection molding PA6/6. |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | ISO Test |
BASF Ultramid® NBX-0025 NF2001 PA66 (Dry) Ultramid NBX-0025 NF2001 is a specialty, unfilled PA6/6. |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | ISO Test |
BASF Ultramid® 1000-11 NF2001 PA66 (Dry) Ultramid 1000-11 NF2001 is a general purpose nylon 6/6. |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | ISO Test |
BASF Ultramid® 1000-2 NF2001 PA66 (Dry) Ultramid 1000-2 NF2001 is a general purpose PA6/6. |
|||
Izod Impact, Notched (ISO) | 5.20 kJ/m² | 2.47 ft-lb/in² | ISO Test |
BASF Ultramid® 1003-2 NF2002 PA66 (Dry) Ultramid 1003-2 NF2002 is a general purpose, heat stabilized nylon 6/6. |