Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 3.15 kJ/m²

@Temperature 22.8 °C
1.50 ft-lb/in²

@Temperature 73.0 °F
ISO 180/1A
Polymer Resources NY66-GP2 General Purpose Nylon 66, Nucleated
General Purpose Nylon 66, Nucleated Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry..
Izod Impact, Notched (ISO) 3.15 kJ/m² - NB
1.50 ft-lb/in² - NB
Average value: 13.3 kJ/m² Grade Count:104
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Izod Impact, Notched (ISO) 3.15 kJ/m²
1.50 ft-lb/in²
Complete Break; ISO 180/B
ExxonMobil Exxtral™ CMW 402 Performance Polyolefin
Product Description: A specialty thermoplastic polyolefin resin designed for automotive under-the-hood applications. Availability: Africa & Middle East, Asia Pacific, Europe, South America and North..
Izod Impact, Notched (ISO) 3.15 - 52.5 kJ/m²
1.50 - 25.0 ft-lb/in²
Average value: 34.3 kJ/m² Grade Count:7
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..