Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 0.450 - 9.50 kJ/m² | 0.214 - 4.52 ft-lb/in² | Average value: 5.65 kJ/m² Grade Count:23 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Izod Impact, Notched (ISO) | 0.450 kJ/m² @Temperature 23.0 °C |
0.214 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |