Polymer Property : Izod Impact, Unnotched (ISO) = 5.00 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 10.5 - 60.0 kJ/m²

@Temperature -40.0 - 30.0 °C
5.00 - 28.6 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 39.6 kJ/m² Grade Count:12
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15..