Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 10.5 - 60.0 kJ/m² @Temperature -40.0 - 30.0 °C |
5.00 - 28.6 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 39.6 kJ/m² Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |