Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 10.5 - 60.0 kJ/m² @Temperature -40.0 - 30.0 °C |
5.00 - 28.6 ft-lb/in² @Temperature -40.0 - 86.0 °F |
Average value: 39.6 kJ/m² Grade Count:12 |
Overview of materials for Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 20% Glass Fiber Filled". Specific grades with glass content between 15.. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 60.0 kJ/m² @Temperature -40.0 - -30.0 °C |
14.3 - 28.6 ft-lb/in² @Temperature -40.0 - -22.0 °F |
Average value: 47.3 kJ/m² Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled". Specific grades with glass content between 25.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 60.0 kJ/m² | 9.52 - 28.6 ft-lb/in² | Average value: 41.5 kJ/m² Grade Count:19 |
Overview of materials for Polyetheretherketone, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Carbon Fiber Filled". Each property range of values reported is minimum and maximu.. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 60.0 kJ/m² | 9.52 - 28.6 ft-lb/in² | Average value: 39.8 kJ/m² Grade Count:4 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Izod Impact, Unnotched (ISO) | 55.0 - 60.0 kJ/m² @Temperature -30.0 - -30.0 °C |
26.2 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 57.5 kJ/m² Grade Count:2 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS)/Nylon Blend". Each property range of values reported is minimum an.. |
|||
Izod Impact, Unnotched (ISO) | 45.0 - 60.0 kJ/m² @Temperature -30.0 - -30.0 °C |
21.4 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 53.8 kJ/m² Grade Count:2 |
Overview of materials for Nylon 66, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum .. |
|||
Izod Impact, Unnotched (ISO) | 30.0 - 60.0 kJ/m² | 14.3 - 28.6 ft-lb/in² | Average value: 47.2 kJ/m² Grade Count:10 |
Overview of materials for Nylon 66, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and ma.. |
|||
Izod Impact, Unnotched (ISO) | 45.0 - 60.0 kJ/m² @Temperature -30.0 - -30.0 °C |
21.4 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 52.5 kJ/m² Grade Count:3 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Izod Impact, Unnotched (ISO) | 20.0 - 60.0 kJ/m² @Temperature -30.0 - -30.0 °C |
9.52 - 28.6 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 38.7 kJ/m² Grade Count:21 |
Overview of materials for PBT + PET Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "PBT + PET Blend, Glass Filled". Each property range of values reported is minimum and maximum values of .. |