Polymer Property : Izod Impact, Unnotched (ISO) = 21000 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 20.0 - 21000 kJ/m²
9.52 - 9990 ft-lb/in²
Average value: 54.3 kJ/m² Grade Count:46
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..