Mechanical Properties Metric English Comments
Adhesive Bond Strength 22.0 MPa

@Temperature -55.0 °C
3190 psi

@Temperature -67.0 °F
Lap Shear
Henkel Hysol AL 2000 Primer
Heat-curing, nitrile phenolic, water-based primer. Cured product furnishes excellent resistance to chemicals and water. Qualified to Boeing BMS 5-42, Type 3.Applications: Sprayable Low Viscosity We..
Adhesive Bond Strength 22.0 MPa

@Temperature 177 °C
3190 psi

@Temperature 351 °F
Lap Shear
Henkel Hysol EA 9689 Film Adhesive
Modified epoxy film adhesive with high temperature strength and long-term thermal durability. Data from 0.10 psf, 500 g/m2.Applications: Composite Bonding Metal and Honeycomb Bonding