Henkel Hysol AL 2000 Primer

Category Polymer , Thermoset , Phenolic
Manufacturer Henkel
Trade Name Hysol
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Henkel Hysol AL 2000 Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Heat-curing, nitrile phenolic, water-based primer. Cured product furnishes excellent resistance to chemicals and water. Qualified to Boeing BMS 5-42, Type 3.Applications: Sprayable Low Viscosity Wet Lay-up Metal and Honeycomb Bonding
Physical Properties Metric English Comments
Storage Temperature 5.00 °C
41.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 10.0 MPa

@Temperature 121 °C
1450 psi

@Temperature 250 °F
Lap Shear
22.0 MPa

@Temperature -55.0 °C
3190 psi

@Temperature -67.0 °F
Lap Shear
29.0 MPa

@Temperature 25.0 °C
4210 psi

@Temperature 77.0 °F
Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Processing Properties Metric English Comments
Cure Time 90.0 min

@Temperature 157 °C
1.50 hour

@Temperature 315 °F
Descriptive Properties Value Comments
Out-Time (days) 30
at 25°C
Primer Coverage, sq.m/L 212
at 8µm dry film thickness