Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 22.0 MPa @Temperature -55.0 °C |
3190 psi @Temperature -67.0 °F |
Lap Shear |
Henkel Hysol AL 2000 Primer Heat-curing, nitrile phenolic, water-based primer. Cured product furnishes excellent resistance to chemicals and water. Qualified to Boeing BMS 5-42, Type 3.Applications: Sprayable Low Viscosity We.. |
|||
Adhesive Bond Strength | 22.0 MPa @Temperature 177 °C |
3190 psi @Temperature 351 °F |
Lap Shear |
Henkel Hysol EA 9689 Film Adhesive Modified epoxy film adhesive with high temperature strength and long-term thermal durability. Data from 0.10 psf, 500 g/m2.Applications: Composite Bonding Metal and Honeycomb Bonding |