Material Notes:
Fast-set fairing and smoothing compound for exterior aircraft surfaces.Sandable after 6 hours
Physical Properties Metric English Comments
Storage Temperature 25.0 °C
77.0 °F
Mechanical Properties Metric English Comments
Adhesive Bond Strength 4.80 MPa

@Temperature 93.0 °C
696 psi

@Temperature 199 °F
Tensile Lap Shear
13.8 MPa

@Temperature -55.0 °C
2000 psi

@Temperature -67.0 °F
Tensile Lap Shear
15.2 MPa

@Temperature 25.0 °C
2200 psi

@Temperature 77.0 °F
Tensile Lap Shear
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 71.0 °C
160 °F
Processing Properties Metric English Comments
Cure Time 60.0 min

@Temperature 71.0 °C
1.00 hour

@Temperature 160 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30 min
30 min
Descriptive Properties Value Comments
Consistency Thixotropic
Form 2 parts
Mix Ratio, Part A:Part B 100:50
Peel Strength Nil