Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Charpy Impact Unnotched = 2.80 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
Plastcom SLOVALEN PH 72 T 40 PP, 40% mineral filling
FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, thermo stable, chemically modified talc. General application in all industry branches - covers of..
Charpy Impact Unnotched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
Radici Radilon® A CV300LK (dry) Nylon 66
Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov..
Charpy Impact Unnotched 2.80 J/cm²

@Temperature -20.0 °C
13.3 ft-lb/in²

@Temperature -4.00 °F
Plastcom SLOVAMID 6 T 30 TS PA6, 30% mineral filling
FeaturesDecreased shrinkage against the BT types, increased heat application. Increased modulus in tension - strength of the material. PA matrix reduction. PA for injection moulding with the content..
Charpy Impact Unnotched 2.80 J/cm²

@Temperature -20.0 °C
13.3 ft-lb/in²

@Temperature -4.00 °F
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As..
Charpy Impact Unnotched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Styrolution Luran® S KR 2858 GS Colored 15% Glass Filled ASA
Description: Glass-reinforced grade with high stiffness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Charpy Impact Unnotched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
80x10x4mm; ISO 179/1fU
SYNTHOS Krasten® 171 General Purpose Polystyrene
Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high ..
Charpy Impact Unnotched 2.80 J/cm²

@Temperature 23.0 °C
13.3 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eU
Sax Polymers SAXALEN PPH121GK30 Polypropylene Homopolymer, 30% Glass Filled
SAXALEN PPH121GK30 is a 20% glass-fiber and 10% glass-beads filled Polypropylene - Homopolymer intended for injection molding. This type has a higher stiffness and a optimized warpage grade.Informat..